Patent
US 10,230,111binder
graphene oxide
N/C element ratio (claimed range, claim 2) | — | graphene powder |
ID/IG ratio (claimed range, claim 3) | — | graphene powder |
powder resistivity (claimed range, claim 4) | — | graphene powder |
O/C element ratio preferred range (description) | — | graphene powder |
N/C element ratio further preferred range (description) | — | graphene powder |
BET specific surface area preferred range (description) | — | graphene powder |
Duration | 15–300 seconds | — |
Duration | 30–60 seconds | — |
Temperature | 25–50 °C | — |
Duration | 0.2–5 hours | — |
Temperature | 80–100 °C | — |
Duration | 5–50 minutes | — |
Duration | 1–30 minutes | — |
Thickness | 0.001 cm | — |
binder
graphene oxide
N/C element ratio (claimed range, claim 2) | — | graphene powder |
ID/IG ratio (claimed range, claim 3) | — | graphene powder |
powder resistivity (claimed range, claim 4) | — | graphene powder |
O/C element ratio preferred range (description) | — | graphene powder |
N/C element ratio further preferred range (description) | — | graphene powder |
BET specific surface area preferred range (description) | — | graphene powder |
Duration | 15–300 seconds | — |
Duration | 30–60 seconds | — |
Temperature | 25–50 °C | — |
Duration | 0.2–5 hours | — |
Temperature | 80–100 °C | — |
Duration | 5–50 minutes | — |
Duration | 1–30 minutes | — |
Thickness | 0.001 cm | — |
binder
graphene oxide
N/C element ratio (claimed range, claim 2) | — | graphene powder |
ID/IG ratio (claimed range, claim 3) | — | graphene powder |
powder resistivity (claimed range, claim 4) | — | graphene powder |
O/C element ratio preferred range (description) | — | graphene powder |
N/C element ratio further preferred range (description) | — | graphene powder |
BET specific surface area preferred range (description) | — | graphene powder |
Duration | 15–300 seconds | — |
Duration | 30–60 seconds | — |
Temperature | 25–50 °C | — |
Duration | 0.2–5 hours | — |
Temperature | 80–100 °C | — |
Duration | 5–50 minutes | — |
Duration | 1–30 minutes | — |
Thickness | 0.001 cm | — |
binder
graphene oxide
N/C element ratio (claimed range, claim 2) | — | graphene powder |
ID/IG ratio (claimed range, claim 3) | — | graphene powder |
powder resistivity (claimed range, claim 4) | — | graphene powder |
O/C element ratio preferred range (description) | — | graphene powder |
N/C element ratio further preferred range (description) | — | graphene powder |
BET specific surface area preferred range (description) | — | graphene powder |
Duration | 15–300 seconds | — |
Duration | 30–60 seconds | — |
Temperature | 25–50 °C | — |
Duration | 0.2–5 hours | — |
Temperature | 80–100 °C | — |
Duration | 5–50 minutes | — |
Duration | 1–30 minutes | — |
Thickness | 0.001 cm | — |